this post was submitted on 24 Jun 2024
440 points (97.8% liked)

Asklemmy

43464 readers
760 users here now

A loosely moderated place to ask open-ended questions

Search asklemmy ๐Ÿ”

If your post meets the following criteria, it's welcome here!

  1. Open-ended question
  2. Not offensive: at this point, we do not have the bandwidth to moderate overtly political discussions. Assume best intent and be excellent to each other.
  3. Not regarding using or support for Lemmy: context, see the list of support communities and tools for finding communities below
  4. Not ad nauseam inducing: please make sure it is a question that would be new to most members
  5. An actual topic of discussion

Looking for support?

Looking for a community?

~Icon~ ~by~ ~@Double_A@discuss.tchncs.de~

founded 5 years ago
MODERATORS
 
you are viewing a single comment's thread
view the rest of the comments
[โ€“] cooltrainer_frank@lemmy.world 210 points 3 months ago (21 children)

Former process engineer in an aluminum factory. Aluminum foil is only shiny on one side and duller on the other for process reasons, not for any "turn this part towards baking, etc" reasons.

It's just easier to double it on itself and machine it to double thickness than it is to hit single thickness precision, especially given how much more tensile strength it gives it.

Also, our QA lab did all kinds of tests on it to settle arguments. The amount of heat reflected/absorbed between the two sides is trivially small. But if you like one side better you should wrap it that way, for sure!

[โ€“] cooltrainer_frank@lemmy.world 7 points 3 months ago (3 children)

Okay, my buddy is gonna take foil tomorrow and run it over the profilometer (?) tomorrow and see. I'll report back with more numbers and less hand waving when I have it

[โ€“] ICastFist@programming.dev 4 points 3 months ago

I'll be here to read those numbers