You can see where around corners and even some straight runs it is peeling up. I'm running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I've trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

you are viewing a single comment's thread
view the rest of the comments
[–] BingoBangoBongo@midwest.social 3 points 8 months ago

Increasing temp by 5, plus recleaning the bed, plus doing some cold pulls helped a bit. I've always had issues getting things to stick at 60 for some reason, at least ever since I went to borosilicate. I'll try adding more squish, since I have to dehydrate my filament before I give the print another shot.