this post was submitted on 15 Jul 2023
17 points (100.0% liked)

3DPrinting

15250 readers
30 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I've read in several places that using back off speeds and clean nozzles can help. I'm running with a new nozzle. Travel speed 150, retraction speed of 20, print speed 50. I think some of these are just defaults with cura 5.4 but I get the same thing with a higher retraction speed. What else should I look at?

you are viewing a single comment's thread
view the rest of the comments
[–] Finite@lemmy.world 1 points 1 year ago (1 children)

I hadn't heard of the temperature tower, thank you

[–] rambos@lemmy.world 1 points 1 year ago

Yeah mate thats super usefull 1st print for every new filament. Temp tower, flow tower, retraction tower and you are set.

Btw calibrating retraction is not just changing speed, you need to find speed and distance. But yeah like others said, your petg probably needs to be dried first