this post was submitted on 28 Jul 2023
23 points (100.0% liked)

3DPrinting

15595 readers
22 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I'm trying to diagnose what tuning I need to get a smooth top layer on a solid print.

The picture you see is a 50mmx50mmx1mm square (cube([50,50,1]); in openscad) printed with a .4 nozzle. (5 layers)

For tuning on the problem, I have looked into:

  • z_offset -- tried all kinds of values and if I reduce it anymore, it doesn't squish into the bed and the center part is exactly 1mm -- so unlikely to be that.
  • bed level -- bltouch is working well
  • extrusion (esteps or rotational_distance) - played with this a great deal and any less and i start to have under-extrusion in the center area.
  • different filament -- same with PLA, PETG and ABS
  • Different slicer -- same with PrusaSlicer or Cura
  • Different speeds -- one on the left was printed at 20mm/s -- the right was printed at 150mm/s

I also cant find any guides out there that show this issue. Anybody with some suggestions or threads I can pull?

you are viewing a single comment's thread
view the rest of the comments
[–] tenzen@lemmy.ca 1 points 1 year ago

Thank you everybody for leading me on the right path.

As I had already installed Klipper, I decided to try the pressure advance calibration as suggested and it did take some tuning, but has improved quality immensely.

In the end, here are the settings I changed: Klipper printer.cfg pressure_advance: 0.120

PrusaSlicer:PrinterSettings:Extruder 1:Retraction Length: 0

I still think I can tweak my z-offset and temperature and maybe further refine pressure_advance, but the results are quite a bit better than before.

I used the Klipper guide for pressure advance: https://www.klipper3d.org/Pressure_Advance.html

Original print on the left, print with the above changes on the right.

Having said that, I think I might have been able to improve the results using a marlin firmware and working with my retraction setup -- I use a non-default direct-drive extruder so the default settings of about 6mm are certainly incorrect.

Also, into the future, i'll check out the wear/maintenance on the nozzle -- it is a good point and I havent changed it in quite a few prints.

Thank you everybody!