this post was submitted on 04 Sep 2023
25 points (96.3% liked)

3DPrinting

15607 readers
242 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I'm thinking of building a new printer and would love to be able to make 2 color prints or dissolvable supports. Does anyone have any experience with this. I see 3 paths.

  1. Two hot ends Pros: Most robust No retraction or filament waste Cons: Alignment issues. Reduced travel Dragging nozzle

  2. Dual filament hot end(taichi style) Pros: Easy to mount No offsets Cons: Jamming? Long retraction

  3. Y splitter Pros: easy to mount No offset Compatible with any hot end Cons jamming Super long retraction

you are viewing a single comment's thread
view the rest of the comments
[–] EmilieEvans@lemmy.ml 1 points 1 year ago (1 children)

2 is mixing hotends. What you describe is 3 (y-splitter with the splitting integrated into the heat sink). They suffer basically the same issues like an "external" y-splitter. You can get them to work but changing materials requires you to do all of the painful setup/calibration once more.

.

That they don't have oozing issues is correct but I never mentioned this in the first place.

.

The main issue with 2 (mixing) is cooking the filament and slicers aren't great at this (operational challenge). There are more pro and cons but I think in the end it boils down to two applications: 1. cheap to integrate. 2. While they are advertised as mixing hotend the result is on pair with dual color/extrusion filament.

[–] shitescalates@midwest.social 1 points 1 year ago

No offense, but I made the list and didn't include mixing hot ends.